NANOINDENTATION

Subject

Browse all works related to NANOINDENTATION.

"7" Result

The launch of silicone hydrogel contact lenses has led to a rise in the incidence of mechanically-related clinical complications, which is thought to be due to the increased stiffness of these materials compared to conventional hydrogel lens materials. The mechanical characteris…